FLEXIBLE POLYESTER

 

HTP-402-99

RATIO:  100pbw to 1/4%-2%pbw

HARDENER:  M.E.K. PEROXIDE

GENERAL DESCRIPTION:  HTP-402-99 is a flexible, low reactivity, low viscosity polyester.  It has very good flow and air release for R.T.M. and hand lay-ups.

 

TYPICAL PHYSICAL PROPERTIES

Ratio by Weight 100 pbw to 1/4%-2% pbw
Viscosity 100-200 cps
Gel Time 35-45 minutes
Cure Time Approximately 12-18 hours
Shore "D" 60
Density 9.0
Specific Gravity 1.08
Shelf Life 3 months