MULTI-PURPOSE CASTING RESIN

 

MCR-507

RATIO:  100pbw to 10 pbw

HARDENER:  HT-106-3

GENERAL DESCRIPTION:  MCR-507 is a tough, hard carbide filled casting material designed for surface facings of Kirksite Dies.  This epoxy system is an exceptional material for applications requiring wear and has abrasion resistance.  MCR-507 features accurate detail and reproduction.

NOTE:  This system must be post cured after the initial room temperature cure, otherwise the system will be very brittle for at least 3-5 weeks.

 

TYPICAL PHYSICAL PROPERTIES

Ratio by Weight 100pbw to 10pbw
Ratio by Volume 5.4 to 1
Pot Life at 72ºF (200 gram mass) 50 minutes
Cure Time 24 hours
Shore "D" Room Temperature 89
Shore "D" 350ºF 78
Heat Distortion 375ºF
Density Resin 14.5
Density Hardener 7.8
Density Mixed 13.9
Specific Gravity Resin 1.75
Specific Gravity Hardener .94
Specific Gravity Mixed 1.68
Shelf Life Resin/Hardener 1 year
Recommended Post Cure:

     2 hours @ 150ºF

     2 hours @ 250ºF

     4 hours @ 300ºF

After 4 hours @300ºF, shut off oven.  Remove tool when oven is at ambient temperature.


Page Last Modified:  05/01/01